Image result for hdpe pipe welding procedure Ge...

  • 2018-07-04T08:26:16

Image result for hdpe pipe welding procedure Generally speaking, HDPE pipe is butt fused by applying heat to prepared pipe ends and then pushing the pipe ends together with a pre-determined force to make a permanent butt fusion joint. It is a very simple process utilizing a properly sized butt fusion machine for the pipe size to be joined.

Image result for hdpe pipe welding procedure Generally speaking, HDPE pipe is butt fused by applying heat to prepared pipe ends and then pushing the pipe ends together with a pre-determined force to make a permanent butt fusion joint. It is a very simple process utilizing a properly sized butt fusion machine for the pipe size to be joined.

  • 2018-07-04T08:26:16

Have any question or need any business consultation?

Have any question or need any business consultation?

Contact Us
Chat with us